We use essential cookies for the basic functionality of our website, such as remembering your selected language. Embedded content, like YouTube videos, may set additional cookies.

en-USsv-SEde-DEfr-FR

Metal analysis


Since 2005 D-lab is accredited for analyses of steel. The accredited analyses methods are mostly in compliance with ASTM standards, but modified for a wider content scope. We are also accreditated for Brass, Bronze, Pure Copper, Titanium alloys and Carbon in Ferrochromium, Ferromanganese, Ferrosilicone and Carbides.

We can analyse your samples of

Fe-base
Ni-base
Cu-base
Al-base
Co-base
Ti-base

Our advanced analyses equipment, duplicated to ascertain high delivery reliability, contains i a the most advanced spectrometers available on the market. See our equipment.

Fe-base | Ni-base | Cu-base | Al-base | Co-base | Ti-base

 

Fe-base

We are accredited for steel and cast iron (white structure) by SWEDAC according to EN 17025, ASTM standard. Below you can see the accredited substance scopes and reference methods.

The procedure
If the samples are flat, min Ø 30 mm and max Ø 55 mm, the analyses are performed utilizing the equipment best suited to the element in question. A ‘full’ analyses comprises the elements listed below, except O, H, Pb, Bi and Sb. Analyses of C, S and N is made by using combustion analyses and for As, P, B and Al optic spectrometry (spark) is used. All other elements are analysed by x-ray fluorescence.

If the samples are of other dimensions than stated above sample preparations will have to be made to fit the equipment. The preparation can be made by flattening, cutting, diluting, casting and other equipment adaptation methods, to fit the required size. See the Sample preparation headline.

Price list

Explanations
ASTM E 572, Analyses of steel by x-ray spectrometry,
ASTM E 1086 Analyses of steel by optical emission spectrometry,
ASTM E 1999 Analyses of cast iron (white structure) by optical emission spectrometry,
ASTM E 1019 Analyses of C, S, N and O in Steel by combustion and techniques
Analyses of H by fusion technique

Table is valid for sample size min 30 mm in diameter. For other sizes, please contact us.

Table FeElement
Carbon, C
Sulfur, S
Nitrogen, N
*Oxygen, O
*Hydrogen, H
Lead, Pb
Bismut, Bi
Phosphorus, P
Arsenic, As
Aluminum, Al
Boron, B
Silicon, Si
Manganese, Mn
Cromium, Cr
Nickel, Ni
Molybdenum, Mo
Titaniumium, Ti
Niob, Nb
Copper, Cu
Cobalt, Co
Tin, Sn
Tungsten, W
Vanadium V
Iron, FeContent scope %
0,002 - 5,00
0,001 - 0,35
0,0005 - 0,5
0,0001 - 1,2
0,00002 - 0,0500
0,00002 - 0,0015
0,00002 - 0,0003
0,002 - 0,15
0,001 - 0,030
0,001 - 1,3
0,0002 - 0,012
0,01 - 4,0
0,01 - 15
0,01 - 30,0
0,01 - 40,0
0,01 - 8,00
0,003 - 2,00
0,005 - 2
0,01 - 4
0,005 - 16
0,002 - 0,1
0,01 - 17
0,005 - 4
RestMethod/standard
ASTM E1019
ASTM E1019
ASTM E1019
ASTM E1019

RR-validerad
RR-validerad
ASTM E1086
ASTM E1086
ASTM E1086
ASTM E1086
ASTM E572
ASTM E572
ASTM E572
ASTM E572
ASTM E572
ASTM E572
ASTM E572
ASTM E572
ASTM E572
ASTM E572
ASTM E572
ASTM E572Comment.
1 g sample
1 g sample



Other trace elements
*Hg, *Cd, *Se, *Te, *Ag*non-accredited
RR-validated = Round Robin-validated

Reports are provided according to the elements in question. Later addition of other elements may be provided free of charge. Additional elements not included in the table will cause extra cost.

 

Fe-base | Ni-base | Cu-base | Al-base | Co-base | Ti-base

Ni-base

Not an accredited area. Ni-base analyses are mainly performed as analyses of steel. If the samples are flat, min Ø 30 mm and max Ø 55 mm, the analyses are performed utilizing the equipment best suited to the element in question.

If the samples are of other dimensions than stated above sample preparations will have to be made to fit the equipment. The preparation can be made by flattening, cutting, diluting, casting and other equipment adaptation methods, to fit the required size. See the Sample preparation headline.

Price list

Explanations
ASTM 2465mod Analyses of Ni-base alloys by x-ray spectrometry
ASTM 1086mod Analyses by optic emission
ASTM 1019 mod. Analyses of C, S, N and O by combustion and fusion techniques
Analyses of H by fusion technique
For scopes outside specified limit, please inquire. The scopes are reviewed annually by Swedac. The table is due for sample sizes of min Ø 30 mm. For smaller sizes, please contact us.

Table NiElement
Carbon, C
Sulfur, S
Nitrogen, N
Oxygen, O
Hydrogen, H
Lead, Pb
Bismut, Bi
Phosphorus, P
Arsenic, As
Aluminum, Al
Silicon, Si
Manganese, Mn
Cromium, Cr
Iron, Fe
Molybdenum, Mo
Titaniumium, Ti
Niob, Nb
Copper, Cu
Cobalt, Co
Tungsten, W
Vanadium V
Nickel, NiContent scope %
0,002 - 2,00
0,001 - 0,35
0,002 - 0,5
0,0001 - 1,2
0,00001 - 0,0500
0,00002 - 0,0015
0,00002 - 0,0003
0,002 - 0,12

0,001 - 0,5
0,01 - 2,0
0,01 - 2
0,002 - 30,0
0,002 - 35,0
0,01 - 20,00
0,003 - 1,00
0,005 - 4
0,01 - 35
0,005 - 13
0,01 - 4
0,005 - 0,3
RestMethod/standard
ASTM E1019
ASTM E1019
ASTM E1019
ASTM E1019



ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465
ASTM E52465Comment.
1 g sample
1 g sample



Other trace elements
*Cd, *Se, *Te, *Ag*kvalitativ

Reports are provided according to the elements in question (a limited number of elements per alloy). Later addition of other elements may be provided free of charge. Additional elements not included in the table will cause extra cost.
The analyses are made for a limited number of elements per alloy.

 

Fe-base | Ni-base | Cu-base | Al-base | Co-base | Ti-base

 

Cu-base


Cu-base analyses are mainly performed as analyses of steel. If the samples are flat, min Ø 30 mm and max Ø 55 mm, the analyses are performed utilizing the equipment best suited to the element in question.

If the samples are of other dimensions than stated above sample preparations will have to be made to fit the equipment. The preparation can be made by flattening, cutting, diluting, casting and other equipment adaptation methods, to fit the required size. See the Sample preparation headline.

Price list

Explanations
SS-EN 15063 Analyses of Cu-base by x-ray spectrometry,
SS-EN 15079 Analyses of Cu-base by optical emission spectrometry,
ASTM E1019 Analyses of N and O in Cu-base by combustion and fusion techniques
Analyses of H in Cu-base by fusion technique

For scopes outside specified limit, please inquire. The table is due for brass samples with sizes of min Ø 30 mm. For smaller sizes, please contact us.

Table Cu

Element
*Carbon, C
*Nitrogen, N
*Oxygen, O
*Hydrogen, H
*Phosphorus, P
Aluminum, Al
Silicon, Si
Manganese, Mn
Cromium, Cr
Nickel, Ni
Copper, Cu
Tin, Sn
Zink, Zn
Lead, Pb
Iron, Fe
Arsenic, As
Antimon, Sb
Bismut, Bi
Magnesium, Mg

Content scope %
0,002 - 0,010
0,002 - 0,100
0,0001 - 0,2
0,00001 - 0,0500
0,002 - 0,19
0,001 - 12
0,01 - 3,5
0,01 - 3,0
0,006 - 0,2
0,006 - 6,5
55 - 98
0,01 - 12
0,01 - 40
0,01 - 12
0,006 - 6
0,01 - 0,25
0,006 - 0,6
0,006 - 0,25



Method/standard
ASTM E1019mod
ASTM E1019mod
ASTM E1019mod
ASTM E1019mod
(ASTM E1019mod)
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod



Comment
1 g sample
1 g sample

Reports are provided according to the elements in question. Additional elements not included in the table can be done, pending an inquiry. The analyses are made for a limited number of elements per alloy.

* Not an accredited area

Fe-base | Ni-base | Cu-base | Al-base | Co-base | Ti-base

 

Al-base

Not an accredited area.

Explanations
ASTM E1251mod Analyses of Al-base by optical emission spectrometry, OES ASTM E1019mod Analyses of C, S, N, O and (H) (in Al-base) by combustion technology

The table is due for sample sizes of min Ø 20 mm. For smaller sizes, please contact us.

Price list

Table AlElement
Beryllium, Be
Bismut, Bi
Kalcium, Ca
Oxygen, O
Hydrogen, H
Cromium, Cr
Copper, Cu
Iron, Fe
Gallium, Ga
Aluminum, Al
Litium, Li
Magnesium, Mg
Manganese, Mn
Natrium, Na
Nickel, Ni
Phosphorus, P
Lead, Pb
Antimon, Sb
Silicon, Si
Tin, Sn
Strontium, Sr
Titaniumium, Ti
Zink, ZnContent scope %
0,0002 - 0,0070
0,001 - 0,535
0,0002 - 0,025
0,0001 - 1,2 (54%)
0,00001 - 0,0010
0,002 - 4,5
0,001 - 11
0,005 - 1,2
0,001 - 0,020
Rest
0,0005 - 0,005
0,001 - 8,0
0,001 - 1,6
0,0002 - 0,006
0,002 - 3,50
0,002 - 0,01
0,002 - 0,5
0,005 - 0,08
0,01 - 15
0,005 - 0,35
0,005 - 0,1
0,001 - 0,03
0,01 - 9,0Method/standard
ASTM E1019mod
ASTM E1019mod
ASTM E1019mod
ASTM E1019mod
(ASTM E1019mod)
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251mod
ASTM 1251modComment.

Reports are provided according to the elements in question. Additional elements not included in the table requires a separate inquire. The analyses are made for a limited number of elements per alloy.

Fe-base | Ni-base | Cu-base | Al-base | Co-base | Ti-base

 

Co-base

Not an accredited area. Co-base analyses are mainly performed as analyses of steel. If the samples are flat, min Ø 30 mm and max Ø 55 mm, the analyses are performed utilizing the equipment best suited to the element in question.

If the samples are of other dimensions than stated above sample preparations will have to be made to fit the equipment. The preparation can be made by flattening, cutting, diluting, casting and other equipment adaptation methods, to fit the required size. See the Sample preparation headline.

Price list

Explanations
ASTM E572mod Analyses (of Co-base) by x-ray spectrometry,
ASTM E1019mod Analyses of C, S, N, O and (H) (in Co-base) by combustion technology

The table is due for sample sizes of min Ø 30 mm. For smaller sizes, please contact us. With large amount of test, please ask for a quotation.

Table CoElement
Carbon, C
Sulfur, S
Nitrogen, N
Oxygen, O
Hydrogen, H
Lead, Pb
Bismut, Bi
Phosphorus, P
Aluminum, Al
Silicon, Si
Manganese, Mn
Cromium, Cr
Nickel, Ni
Molybdenum, Mo
Titaniumium, Ti
Niob, Nb
Copper, Cu
Cobalt, Co
Tin, Sn
Tungsten, W
Vanadium V
Iron, Fe
Zinc, ZrContent scope %
0,002 - 1,00
0,0005 - 0,003
0,002 - 0,15
0,0001 - 0,20
0,00002 - 0,0500
0,00002 - 0,0015
0,00002 - 0,0003
0,002 - 0,01
0,001 - 1,2
0,01 - 0,6
0,01 - 1,5
0,01 - 35,0
0,002 - 12,0
0,01 - 5,00
0,003 - 0,020
0,005 - 0,2
0,01 - 0,04
Rest
0,002 - 0,01
0,01 - 14
0,005 - 0,1
0,005 - 4,0
0,002 - 0,01Method/standard
ASTM E1019mod
ASTM E1019mod
ASTM E1019mod
ASTM E1019mod
(ASTM E1019mod)
RR-validerad mod
RR-validerad mod
ASTM E1086mod
ASTM E1086mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572mod
ASTM E572modComment.
1 g sample
1 g sample


  

Reports are provided according to the elements in question. Later addition of other elements may be provided free of charge. Additional elements not included in the table will cause extra cost. The analyses are made for a limited number of elements per alloy.

Fe-base | Ni-base | Cu-base | Al-base | Co-base | Ti-base

 

Ti-base

Partly accredited area. Ti-base analyses are mainly performed as analyses of steel. If the samples are flat, min Ø 30 mm and max Ø 55 mm, the analyses are performed utilizing the equipment best suited to the element in question.

If the samples are of other dimensions than stated above sample preparations will have to be made to fit the equipment. The preparation can be made by flattening, cutting and other equipment adaptation methods, to fit the required size. See the Sample preparation headline.

Price list

Explanations
X-ray fluorescents and combustion technology are used for the analyses:
ASTM E 539 X-ray Emission analysis of 6Al-4V Ti-alloy,
ASTM E1447, Determination of Hydrogen in Ti and Ti-alloys by inert Fusion TC/infrared Detection Method,
ASTM E1409 Determination of Oxygen and Nitrogen in Ti and Ti-alloys by Inert gas fusion technique,
ASTM 1941 Determination of Carbon in refractory and Reactive Metals and Their Alloys

Table TiElement
Carbon, C
*Sulfur, S
Nitrogen, N
Oxygen, O
Hydrogen, H
*Lead, Pb
*Bismut, Bi
*Phosphorus, P
*Aluminum, Al
*Silicon, Si
*Manganese, Mn
*Cromium, Cr
*Nickel, Ni
*Molybdenum, Mo
*Titaniumium, Ti
*Niob, Nb
*Copper, Cu
*Cobalt, Co
*Tin, Sn
*Tungsten, W
*Vanadium V
Iron, Fe
*Zinc, ZrContent scope %
0,002 - 0,10
0,0005 - 0,003
0,002 - 0,10
0,0001 - 0,20
0,0001 - 0,025
0,00002 - 0,0015
0,00002 - 0,0003
0,001 - 0,005
0,02 - 7,8
0,005 - 0,08
0,001 - 4,6
0,005 - 3,1

0,01 - 4,8
Rest
0,005 - 0,2
0,001 - 0,04
Rest
0,001 - 2,5

0,005 - 5,6
0,005 - 0,6
0,001 - 4,0Method/standard
ASTM E1941
ASTM E1941mod
ASTM E1409mod
ASTM E1409mod
ASTM E1447mod
RR-validerad mod
RR-validerad mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539mod
ASTM E539modComment.

 

 

 

 

 

 

 

 

 

 

 

The analyses are made for a limited number of elements per alloy.

 




Contact


Box 54
693 21 Degerfors 
Sweden
Phone: +46(0)586-216350
E-mail: [email protected]
VAT nr: SE 556609044401




Packages/Visit


Degerfors Laboratorium AB
Bruksparken
693 32 Degerfors
Sweden




Prices


Our prices are often 50% or more below others prices and nobody is faster than us. Price list




Courses & Consulting


OES-courses, XRF-courses, LECO-courses and Consulting.

Ackreditering